Products

Home 3D printing powder High temperature alloy powder

Nickel based superalloy Nickel Inco718 Alloy Powder used for 3D printing

new products

Latest News

November 2,2026.

SAT NANO to Present Research-Grade Nanomaterials at the 7th China New Materials Industry Development Conference

NANJING, November 2, 2026 — SAT NANO will exhibit at the 7th China New Materials Industry Development Conference, taking place November 4–8, 2026 at the Nanjing International Expo Center. The company will present research-grade nanomaterials — includ...

October 27,2026.

SAT NANO is waiting for you to visit at the 7th China International Plastics Exhibition

The 7th China International Plastics Exhibition 2026, hosted by the China Plastics Processing Industry Association, is about to grandly kick off! The exhibition was founded in 2014 and is held every two years. It has been successfully held six times ...

September 23,2026.

Holiday Notice — Mid-Autumn Festival & National Day

Dear Customers,  Thank you for your ongoing support and trust. Our office will be closed for two upcoming holidays:  · Mid-Autumn Festival — September 25 to 27, 2026  · National Day Holiday — October 1 to 7, 2026  Our mailbox does...

July 21,2026.

SAT NANO Ships 1KG Nano TiO₂ Dispersion to South Korean Client — Purpose-Built for Photocatalytic Applications

Last week, SAT NANO successfully completed an export order to the South Korean market — delivering 1KG of aqueous nano titanium dioxide (TiO₂) dispersion to a Korean company specializing in photocatalytic environmental remediation. The...

July 6,2026.

SAT NANO Supplies 1g Multilayer Ta₄C₃ MXene Powder to a Shenzhen Research Institute — A Custom Research-Grade 2D Material Solution

In June 2026, SAT NANO received an urgent request from a materials science research institute in Shenzhen: 1 gram of high-purity multilayer Ta₄C₃ MXene powder, intended for cutting-edge research on 2D material properties. The institute had clear...

June 4,2026.

Improving internal exciton confinement to prepare efficient blue quantum dot light-emitting diodes based on CdZnSeS

In the field of quantum dot light-emitting diodes (QLEDs), CdSe based quantum dots have been widely studied and have achieved excellent performance in red and green emitting QLEDs. However, to achieve blue luminescence, CdSe nuclei need to become ext...

June 4,2026.

Matrix induced luminescence enhances carbon quantum dots to achieve high-performance heavy metal free electroluminescent diodes

Carbon quantum dot CQDs, as environmentally friendly luminescent materials, typically exhibit high quantum yields under photoluminescence conditions. Traditional CQDs can achieve a photoluminescence quantum yield (PLQY) of over 80% in solution, but P...

May 29,2026.

Pixelated perovskite quantum dot superlattice light-emitting diode

Perovskite quantum dots have the advantages of high color purity, high radiation recombination efficiency, and solution processability, making them naturally suitable for high-end displays and microdisplay devices. However, there is always a bottlene...

May 14,2026.

Conducting hydrogel constructs three-dimensional nano electrode network, electrocatalysis triggers chemotherapy immune synergistic anti-tumor

Electrotherapy strategies have shown great potential in tumor treatment, especially in electrodynamic therapy (EDT) which utilizes platinum based (Pt) nanomaterials to catalyze the production of reactive oxygen species (ROS) under an electric field t...

May 14,2026.

Functionalized nano selenium provides new ideas for tumor rehabilitation

Triple negative breast cancer is characterized by strong invasion, high recurrence rate and poor prognosis due to the lack of expression of estrogen receptor, progesterone receptor and HER2. At present, there is still a lack of effective targeted tre...

Nickel based superalloy Nickel Inco718 Alloy Powder used for 3D printing

Buy Nickel based superalloy Nickel Inco718 Alloy Powder used for 3D printing 0-25um and 15-45um, 45-105um size, 99.9% purity, high quality and good price and fast delivery time, please check the specification.


  • Brand:

    SAT NANO
  • Item NO.:

    Inco718-1U
  • Payment:

    TT, Paypal, WU
  • Product Origin:

    China
  • Color:

    grey Powder
  • Shipping Port:

    Shenzhen, Shanghai
  • Lead Time:

    1-5days
  • Min Order:

    1kg
  • Product Details

Specification of Nickel Inco718 Alloy Powder:

Chemical Composition(%) of Inconel 718 Powder
C
Mn
Si
P
S
Cr
Co
Mo
≤0.08
≤0.35
≤0.35
≤0.015
≤0.015
17-21
≤1.0
2.8-3.3
Nb+Ta
Ti
Al
Fe
Cu
Ni
N

4.75-5.5
0.65-1.15
0.2-0.8
Bal
≤0.03
50-55
≤0.006

Inconel 718  Powder Properties
Size Range
0~25um
0~45um
15~45um
45~105um
75~180um
Morphology
Spherical
Spherical
Spherical
Spherical
Spherical
   
      PSD 
(Particle Size Distribution)
D10: 6um
D10: 9um
D10: 14um
D10: 53um
D10: 78um
D50:16um
D50: 28um
D50: 35um
D50: 69um
D50: 120um
D90: 23um
D90: 39um
D90: 45um
D90: 95um
D90: 165um
Flow ability
N/A
≤30S
≤28S
≤16S
≤18S
Apparent Density
4.2g/cm3
4.5g/cm3
4.4g/cm3
4.5g/cm3
4.4g/cm3
Oxygen Content     (wt % )
O: 0.06~0.018wt% ,  ASTM standard : ≤0.02 wt%
3D printing Gas Atomized Inconel 718 Powder with the best price
(low oxygen , high sphericity and good flowability)

Application of Nickel Inco718 Alloy Powder:

Through the different particle size distribution,Nickel 718 powder can be subdivided into injection molding powder, laser cladding powder, spraying powder, hot isostatic pressing powder and so on..

1.HVOF

2. Plasma coating

3.3D printing

 4.powder welding

 5.metal injection molding

 6.hot isostatic


Storage conditions:
Nickel Inco718 Alloy Powder should be sealed and stored in a dry and cool environment. It should not be exposed to the air for a long time, to prevent agglomeration due to moisture, affecting the dispersion performance and use effect, and should avoid heavy pressure, do not contact with oxidant, and transport according to ordinary goods.

Request A Free Quote
If you are interested in our products and would like to know more,please leave us a message and we will get back to you as soon as possible!
Provide the right solution according to your needs,offer efficient service,leave a message for the product information and requirements you need,customize now!
Related Products
Nickel Inco625 Alloy Powder

In625 Nickel Base Alloy Inconel 625 Powder For 3D printing

Buy In625 Nickel Base Alloy Inconel 625 Powder For 3D printing 0-25um and 15-45um, 45-105um size, 99.9% purity, high quality and good price and fast delivery time, please check the specification.

Spherical stellite 20 cobalt alloy powder

Spherical stellite 20 cobalt alloy powder

Buy Spherical stellite 20 cobalt alloy powder for 3D printing 0-25um and 15-45um, 45-105um size, 99.9% purity, high quality and good price and fast delivery time, please check the specification.

Spherical Hastelloy X alloy powder

Spherical Hastelloy X alloy powder for 3D printing

Buy Spherical Hastelloy X alloy powder for 3D printing, 15-53um, 15-45um, 50-150um size, 99.9% purity, high quality and good price and fast delivery time, please check the specification.

ultrafine niobium powders

high quality ultrafine niobium powders for sale

Size:50nm, 100nm, 1-2um, 5um, Purity:99.9% CAS No:7440-03-1 ENINEC No.:231-143-9 Appearance:light gray powder Shape:Spherical

spherical lanthanum oxide

spherical nanometer La2O3 lanthanum oxide particle 40nm

Size:40nm, 1um Purity:99.9% CAS No:1312-81-8 ENINEC No.:215-200-5 Appearance:white Powder Shape:Spherical

High Entropy Alloy Single layer TiVCrMoC3 MXene powder

High Entropy Alloy Single layer TiVCrMoC3 MXene powder

Buy High Entropy Alloy Single layer TiVCrMoC3 MXene powder,  size 200-1000nm, high quality, low price and fast delivery, if you have any interest, please click it to check the specification.

Germanium dispersion

Supply water liquid dispersion Ge Nanoparticle Germanium dispersion

Buy water liquid dispersion Ge Nanoparticle Germanium dispersion, Size:30-50nm and 100-200nm, solid content:1000ppm, 5000ppm, high quality and low price, if you have any interesting, please feel free to contact us. Purity:99.99%

graphene oxide dispersion

graphene oxide dispersion produced by Hummer method

Buy graphene oxide dispersion produced by Hummer method, particle 5-15nm, graphene oxide 1%, 2%, 5%, please feel free to check the specification

Molybdenum trioxide Nanopowder

high purity 99.99% Molybdenum trioxide Nanopowder 100nm Nanoparticles

Buy high purity 99.99% Molybdenum trioxide Nanopowder 100nm Nanoparticles, Purity:99.9%, 99.99%, high quality and good price and fast delivery time, please check the specification.

Single Layer Tantalum carbide Ta4C3Tx MXene powder

Single Layer Tantalum carbide Ta4C3Tx MXene powder

Buy Single Layer Tantalum carbide Ta4C3Tx MXene powder,  size 200-1000nm, high quality, low price and fast delivery, if you have any interest, please click it to check the specification.

Plastic Antibacterial ZnO

Supply Nano Sized Zinc Oxide Powders used for Plastic Antibacterial Agent

Buy Nano Sized Zinc Oxide Powders used for Plastic Antibacterial Agent , Size 20-30nm, Purity:99.8%, high quality, low price and fast delivery, please click to check the specification

ultrafine Boron powder wholesale

Supply Ultrafine Monomer Boron Amouphous Boron Powders factory price

Buy Ultrafine Monomer Boron Amouphous Boron Powders factory price, Size:100-200nm, 300-500nm, 1-3um, 5um, 10um, 20um Purity:90%-99%, high qaulity, low price and fast delivery, please click it to check the specification.

Leave a message Please click here for inquiry
Provide the right solution according to your needs,offer efficient service,leave a message for the product information and requirements you need,customize now!